Large roll galvanized wire welding net is made of high quality galvanized wire welding net, wire through the current, after mutual melting, strong connection point, and the formation of metal mesh. In the use of galvanized iron wire to find the thickness and soft and hard to the size of flowers, weight and softness corresponding to the degree, too soft florets to use fine wire, and heavy flowers, flowers with thick stems to use thick wire.
Two, the production process is different
Galvanized wire mesh is divided into hot dip galvanized wire mesh and cold galvanized wire mesh. Galvanized steel wire net selects the high quality low carbon steel wire, iron wire factory made by precision of automation machinery welding technology processing, smooth surface, firm structure, integrity is strong, even if the local cutting of galvanized steel wire net, or local also under pressure from loose phenomenon, after molding, wire mesh galvanized corrosion resistance good, has the advantage that the general steel mesh does not have.
- When pickling, we should pay great attention to the acid has a strong corrosion, so when adding acid, we must pour acid into water, and it is along the wall of the cylinder, not a splash down, so as not to cause splash. Remember the order of pouring acid, acid into water rather than water into acid, water into acid will cause splashing and boiling, when pouring acid must wear protective glasses, must ensure that there are no non-professional onlookers, so as not to cause some risk of splashing acid.
Post time: 27-03-23
Post time: 01-08-22
Post time: 02-03-23
Post time: 24-08-22
Post time: 01-11-22- After a long time of use, it will not rust after the corrosion protection layer on the surface of hot dip galvanized barbed rope, because the material inside the stainless steel barbed rope is the same as the material on the surface.
- Galvanized wire to galvanized uniform, a body is now its cross section, the second is the longitudinal uniformity. In the actual operation process, such as the jitter of steel wire, the surface of the pot scum and other reasons will cause galvanized wire surface galvanized layer accumulation, should try to solve the problem.
- Generally larger birds choose tall but more dense cage, so as not to damage the tail feathers. Although bailing and other small body, but high flying singing habits, with a special high cage.
- Five: Spray blade barbed rope specifications: BTO-10, BTO-12, BTO-18, BTO-22, BTO-28, BTO-30, CBT-60, CBT-65
The temperature of large roll galvanized wire should be controlled at 30 to 50℃ during electroplating. Because the chloride ions in the bath are very corrosive, quartz glass heaters are generally used. Continuous production does not need heating, but needs cooling. Cooling can be in the groove side row thin wall plastic pipe, through the flow of tap water cooling, can also be used as a titanium pipe temperature control device.
If the blade barbed rope produced by the barbed rope factory wants to be made into a straight line, it can’t be made too long because of the constraints of logistics.
Post time: 16-11-221. PVC plastic coated barbed rope adopts flexible structure
Abandoned barbed wire guardrail network will generally choose classification pick up, classification gathering pick up and other methods, better to promote the better use of the whole highway guardrail network, abandoned metal guardrail network is still common copper mesh profile.
Compared with traditional braided and twisted braided rope, the process of blade braided rope is relatively complex, and the price of raw materials is also relatively high.
Post time: 26-12-22- Similar to two materials in the coating part melting together, and coating thickness can reach 100 microns, so high corrosion resistance, salt spray test 96h no problem, equivalent to 10 years under the usual environment; Cold galvanizing is electroplating at room temperature. Although the thickness of the coating can also be controlled, the binding strength and thickness of the coating are relatively low, so the corrosion resistance is poor.
Post time: 29-04-22Did not do the adhesion test of powder spraying or fluorocarbon spray on the packaging galvanized wire, but there are two points for reference: one, in the sealed or air circulation environment, non-metallic volatiles can corrosion zinc coating; Second, zinc above 230 degrees (c) will brittle the base metal. After powder spraying and fluorocarbon spraying, it is necessary to bake at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in decreased adhesion of coating, and even leading to brittle situation of steel wire.
Post time: 14-02-23Friends in the industry know that galvanized iron wire has two kinds of cold galvanized iron wire and hot galvanized iron wire, so what is the difference between cold galvanized iron wire and hot galvanized iron wire? Which is good?